Extraction of Bismuth and Antimony by Wet-process From Lead Anode MudChinese Full Text

JIA Hui;WANG Xing;CUI Jia-you;HOU Shao-bin;LIN Hao;Shandong Humon Smelting Co.,Ltd.;

Abstract: Leaching of bismuth and antimony from lead anode mud oxidized at high temperature using hydrochloric acid as leaching agent,ferric chloride as oxidant,sodium chloride to provide more chloride ions was investigated.The effects of oxidizing temperature of lead anode mud,hydrochloric acid concentration,leaching temperature,reaction time,ratio between liquid volume and solid mass,the amount of ferric chloride and sodium chloride on leaching of bismuth and antimony were examined.The experimental results show that the pretreatment for lead anode slime has a greater influence on the leaching of bismuth and antimony.Under the conditions of hydrochloric acid concentration of 5mol/L,ratio between liquid volume and solid mass of 5∶1,leaching temperature of 80 ℃,reaction time of 3h,ferric chloride concentration of 10g/L,sodium chloride concentration of 45g/L,the leaching of bismuth and antimony reach 99.44% and 99.69% respectively for the lead anode mud oxidized at 200℃and through 200 mesh sieve.
  • DOI:

    10.13355/j.cnki.sfyj.2014.05.09

  • Series:

  • Subject:

  • Classification Code:

    TF817;TF818

  • Mobile Reading
    Read on your phone instantly
    Step 1

    Scan QR Codes

    "Mobile CNKI-CNKI Express" App

    Step 2

    Open“CNKI Express”

    and click the scan icon in the upper left corner of the homepage.

    Step 3

    Scan QR Codes

    Read this article on your phone.

  • HTML
  • CAJ Download
  • PDF Download

Download the mobile appuse the app to scan this coderead the article.

Tips: Please download CAJViewer to view CAJ format full text.

Download: 251 Page: 368-370 Pagecount: 3 Size: 266K

Related Literature
  • Similar Article
  • Reader Recommendation
  • Associated Author